This is not "hard facing" rod.
RC 45.
I didn't want my anvil hard to grind, just at least as hard as my hammer.
Not harris/welco.
MG Industries1-800-558-8524
Menomonee Falls, WI
I've been using this secret missle for about 12 years now for surfacing
anvils, and joining diss- steels.
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
From: "Howell Steve" <[email protected]>
To: <[email protected]>
Sent: Tuesday, April 06, 2004 3:54 PM
Subject: [TheForge] trenton fix
> Thanks for the info, Dan.
> I just got back from the weld store with more questions than I had
answered.
>
> Most hardfacing rod they had was the super-abrasion kind (up to 60RC) and
> has a two pass limit.
> Of course, MG750 elicited a 'Whaa...?" response.
>
> Is it made by Harris Welco?
>
> They did have some 'supermissile' from them that is 312SS , designed for
> dissimilar metals.
>
> Time to do more research.
>
> Steve
>
> >>>>>
>
> The best spec says NO PRE-HEAT/ POST-HEAT!
> That was enough for me.
> It is a " highest impact " rod used in the rock crushing industry.
> Peen and work harden. Excellent for tool to mild.
> I don't get a very good color match after rust as this is a high manganese
> rod.
> AC/DC 150 amp. tight arc.
>
>
> dan tull
> georgia
> abba, afc, S.C. psba, obg,sofa
>
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>