Hi Dan,
What's the spec's on it?
I'll see what my welding supplier has here at lunch-time.
The Stoody rod sounds good and forgiving with a 40-50RC rating., good
bonding to carbon steels, etc.
I don't want to go too hard on the filler and the anvil really doesn't need
buildup at all, just some gouges and edge work confined to the face plate.
The horn nicks I'm going to go after with 6010 or 11.
I tried looking up UTP's site to cross-reference some stuff but their site
didn't seem as friendly.
Steve
>>>>
Try MG750!