Bruce:
I'd respectfully argue that a hard face on a treadle hammer is not
desirable. A softer face will "stick" to a struck tool allowing greater
latitude in alignment. With a hard face, more struck tools go flying to
mysterious locations where they hide for years. Pete F
Bruce Freeman wrote:
>I'm designing another treadle hammer, a lightweight job. I want the ram
>to be 20#. What would be ideal is square or roundstock of about 2
>sq.in. in cross-section (i.e., 2" square or 2.25" round) and about 18"
>long.
>
>Ideally, the material would be suitable for use as a hammer, with
>ordinary hardening & tempering. Exotic materials not needed, but mild
>steel wouldn't be appropriate unless faced with tool steel (a
>possibility I'd prefer to avoid).
>
>Since I prefer to design in scroungeable materials, I could use some
>suggestions as to sources of such steel. The truck axles I've seen are
>of smaller diameter than this (though I've seen tractors with axles of
>3" dia.). Track pins seem to be shorter than this - like 8" or so.
>Anyone have any other suggestions - preferably of materials you'd have
>no particular trouble scrounging yourself?
>
>Thanks in advance,
>
>Bruce
>NJ
>
>
>
>
>
>
>
>--- StripMime Report -- processed MIME parts ---
>multipart/alternative
> text/plain (text body -- kept)
> text/html
>The reason this message is shown is because the post was in HTML
>or had an attachment. Attachments are not allowed. To learn how
>to post in Plain-Text go to: http://www.expita.com/nomime.html ---
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>
>
>