We made on recently from three pieces of plate. The middle piece was 1/4
" smaller than the outer two. The shape was a right angle with the "
hypotunuse" leg curved in. The three pieces were riveted together. The
outer two had a small bend out where they met the chandelier. The effect
was a heavier arm ,with a slot at the top where the wire was hidden.
 I'll find a photo and post it. Bob
----- Original Message -----
From: "lama" <[email protected]>
To: "TheForge" <[email protected]>
Sent: Wednesday, June 18, 2003 1:31 AM
Subject: [TheForge] chandelier arms


I am working out the details for a commission to make two chandeliers
similar in design. One is 48" dia. round shape the other is 48" x 24"
dia oval shape. These are typical elegant pieces with long spindly arms.
I am wondering what to make the arms from? Seems like 1/8" or 1/4" black
iron pipe would be too......clunky. Any ideas welcome.
Dave Mudge

--- StripMime Report -- processed MIME parts ---
multipart/alternative
  text/plain (text body -- kept)
  text/html
The reason this message is shown is because the post was in HTML
or had an attachment.  Attachments are not allowed.  To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html  ---
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________