> I am a bladesmith and I use those pieces of scrap steel some would
scoff at
> and my blades come out very good I want to tell you.Yes I have had
some that
> I have gotten to that almost finished stage and found the hairline
cracks of
> stress in them and when I do it gets tossed and goes no further.I
for one
> really like the fact that my blades are from recycled materials.In
this day
> and age of waste I find many of the folks buying my knives like that
fact
> that it used to be a coil spring from a car or truck or was cut from
an old
> saw mill blade and I have remade it into a working tool.
> I have also made power hammer tools from old spring stock and have
had no
> problems with it.The key is how it is heat treated and this is what
makes all
> the
> difference.
>
> Bob
> HotAnvil Forge
> http://members.tripod.com/hotanvil_forge
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>