[TheForge] Rust Patina Finish
gblacksmith
[email protected]
Sun Aug 10 21:41:01 2003
Kevin: Chlorine bleach? That would certainly be a strong oxidizer.....Hmm.
I have used a commercial plum brown on a .50 Hawken kit I built..it works
well on most kit barrels. Was your faux rust finish a commercial
preparation/colorant?
Grant
----- Original Message -----
From: "Kevin donahoe" <[email protected]>
To: <[email protected]>
Sent: Sunday, August 10, 2003 5:49 PM
Subject: RE: [TheForge] Rust Patina Finish
> Grant,
>
> I was at a fellows shop that antiques muzzleloaders. He said he boiled
the
> barrels in bleach, outdoors of course. They had deep etches in them, not
to
> my liking, but then...
>
> I've also been successful doing a faux rust finish for interior work.
Kevin
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of Clyde Wynia
> Sent: Sunday, 10 August, 2003 8:29 AM
> To: [email protected]
> Subject: RE: [TheForge] Rust Patina Finish
>
>
> >All Hands: Does anyone out there have any experience with rust
patination
> of mild steel? I would like to try this finish on a large >piece, have
not
> tried it before and would be interested in hearing the experiences of my
> fellows on this finish.
>
> I make and rust over 1000 pieces of sculpture every year ranging from
small
> pieces to some 15 feet tall. I remove the mill scale either with
> sandblasting or a dilute solution of muriatic acid. Then a mixture of 1
pint
> hydrogen peroxide, 1/cup vinegar, and 13 cup of salt is sprayed on. The
rust
> starts to form immediately and within an hour or less the piece looks
> rusted. I rinse it after any aware from an hour to 12 hrs. It continues to
> rust quite fast.
>
> For some folks tell them to come back in an hour and I will have a piece
> rusted for them. They are very happy to come back an hour or two later and
> see what was a black mill scaled piece now all rust. Of course it is not a
> very deep rust, but it looks good and will continue to deepen, especially
in
> rainy or high humidity weather.
>
> If you don't rinse it, it will turn what I consider a very ugly blackish
> rust.
>
> Clyde Wynia
> Marshfield, WI
> http://www.jurustic.com
>
>
>
>
>
>
> Grant
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>