[TheForge] 36 diameter ring
[email protected]
[email protected]
Wed Aug 6 00:40:00 2003
About that weld; you're aiming to have it come out the same thickness as
the rest of the circle, so there's no adding or subtracting involved=2E Yo=
u
cut it to the right length, upset, scarf, weld, hammer it out, and it come=
s
out perfect every time, no?
Andy G=2E
"Last question is the rule of thumb for final length of the stock in order=
to
forge-weld the ring together=2E"
--------------------------------------------------------------------
mail2web - Check your email from the web at
http://mail2web=2Ecom/ =2E