Check with Richard Furrer. He uses it for his flux. I have had extreme
success using a combination of 1 part boric acid and 4 parts borax. It is
less toxic than using Sal Ammoniac and works very well.
Bill
----- Original Message -----
From: "Brian Gilbert" <[email protected]>
To: <[email protected]>
Sent: Wednesday, September 18, 2002 7:31 PM
Subject: [TheForge] Re:Sal Ammoniac for flux
> OK, folks, here's a puzzler...
>
> Does anyone know of a cheap source of or common use for sal ammoniac
> (ammonium chloride)? I want to use some to blend up my own flux, but
> everything that I've found so far is more expensive than commercial
welding
> flux.
>
> The only common use that I've found so far is for stained glass workers.
I'm
> sure it's probably some sort of cleaning powder, but I'm not sure.
>
> any ideas?
>
> Thanks
> BG
>
> --
> Brian Gilbert
> Editor, The Hammer's Blow
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>