[TheForge] Re:Sal Ammoniac for flux
[email protected]
[email protected]
Wed Sep 18 21:22:01 2002
In a message dated 9/18/2002 8:37:35 PM Eastern Daylight Time,
[email protected] writes:
> Does anyone know of a cheap source of or common use for sal ammoniac
> (ammonium chloride)?
Brian, have you tried a chemical supply house? Ammonium Chloride is pretty
cheap in bulk volume. You may be able to buy a lifetime supply for what
you'd pay for a couple of solid tinning blocks of sal ammoniac.
Mike