[TheForge] Painting Cast Aluminum fountain for outdoors

Dan Tull [email protected]
Wed Oct 16 13:33:01 2002


CleanX3

Phosphoric etch, zinc chromate primer, several top coats.
Consider chlorated rubber based epoxy.
----- Original Message -----
From: "Ken Showalter" <[email protected]>
To: <[email protected]>
Sent: Wednesday, October 16, 2002 1:16 PM
Subject: [TheForge] Painting Cast Aluminum fountain for outdoors


> Just got a 3-tier aluminum fountain which will be installed as the Peace
Fountain at my wife's school.
> It comes unpainted and rough(from Mexico) and after I grind it smooth am
going to paint it black.
> My thought is to prime it with metal primer and use several coats of epoxy
paint. Any suggestions?
> Thanks-Ken
>
>
>
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed.
> Please post in Plain-Text only.---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>
>