[TheForge] Brazing vs welding
[email protected]
[email protected]
Fri Nov 15 12:10:02 2002
For many applications it is a matter of equipment availability and preference. Brazing is slower in many cases and puts more heat into the work piece much of the time.
You may notice I have a preference for welding. For non-ferrous I like brazing over TIG in many cases.
IMHO
Ray
Cincinnati
>
> From: Dave Brown <[email protected]>
> Date: 2002/11/14 Thu PM 03:54:44 EST
> To: TheForge <[email protected]>
> Subject: [TheForge] Brazing vs welding
>
> I've been looking around and reading and have started to think that maybe
> I'm welding too often (forge and/or MIG and/or stick) and maybe should do
> more brazing in certain applications. I found one good site on line that
> tells a lot about brazing, it's pros and cons. It is The Brazing Book
> online and can be found at
> http://www.handyharmancanada.com/TheBrazingBook/contents.htm#Index
>
> There seems to be a lot more versatility and strength to brazing than I
> thought. I think this online book on brazing is gonna be worth a little
> more reading/browsing.
>
> Anyone have any thoughts or experience to share on brazing in the forge?
>
>
> Dave Brown
> Heritage Smithing
> Green Bay, WI
> ABANA, UMBA, GoM, MODA, ARG
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>