[TheForge] Mastermyr

Ralph [email protected]
Tue May 28 21:14:01 2002


To be honest I am not sure as to the strip that is referred to. The text is 
from the book. But it could be the center strip. Perhaps. If the center 
strip were two separate pieces as they look like that were riveted together.
But I am not sure.

Ralph

At 10:59 AM 5/28/02 -0400, you wrote:
>Ralph,
>
>Follow all your dimensions but the "strip width 0.45 cm, thickness 0.25 
>cm"   What's this referring to?  If its the center strip the dimensions 
>don't seem right.   From the pictures and sketches the center strip 
>between the grid rods appears wider and thinner than the grid rods. Am 
>planning on making these 2 strips 3/4" by 1/8" (That would be 1.9 cm by .3 cm)
>
>Ralph wrote:
>
>>I hope this helps.
>>
>>Frame about 50 X 50 cm: strip width 0.45 cm, thickness 0.25 cm; grid rods 
>>49.0 X 1.2 X 0.3-0.5 cm.
>>Chain links about 0.6-0.7 cm, total length of each chain about 42 cm. 
>>Swivel: four-armed plate
>>about 16 X 9 cm, thickness 0.3 cm; hook 10.3 X 1.5 X 0.7 cm; the open 
>>part of the hook maximum
>>width 1.5 cm.
>
>"Good is the enemy of Excellent. Talent is not necessary for Excellence.