George,
Sounds like something worth trying out. Who isthe supplier, or where can
one get some?
Ray Miller
Cincinnati
George Dixon wrote:
> There is a material sold under the name Ceramit. It is a two part
> "synthetic enamel", available in many colors. The two parts are
> mixed, the material is set into or onto whatever you want 'enameled'
> and then it is fired in ann electric stove at 200 degrees. The result
> looks like traditional enamel and is within one rockwell point of
> fired glass enamel. I have used it on bronze and steel.
>