[TheForge] finish help

Dave Brown [email protected]
Tue Jan 8 16:37:00 2002


Jon,

Do you know if the spray galvanizing paints qualify, or does it have to be 
a plating or hot dip application of zinc?

Dave

At 16:15 01/08/02, you wrote:
>i have to say that i would recommend against a powder coat....
>they really don't hold up that well to higher temp ranges 350f and
>above....... (these are the temps use to set them)
>also on steel powder coating without a zinc deposition layer will not really
>give you a good rust proofing (or bond for that matter as rust developing
>under the coat will peel it like a bananna) the zinc coat would ruin any
>surface coloring you would have...... (looks just like thick
>galvanization.....)
>
>anywho just my 2 pennies on that one.........
>
>jon p