[TheForge] Help! finish problem
H and P Foster
[email protected]
Thu Feb 7 03:19:08 2002
It drys in my shop (not too warm) and I just brush on a coat, not thick, not
thin. I think you might not have enough Japan dryer in your formula.
Harry Foster
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of northwoods
Sent: Wednesday, February 06, 2002 7:57 PM
To: [email protected]
Subject: Re: [TheForge] Help! finish problem
Under what conditions do you have it drying? How thick of a coat did you put
on?
T. Clark
----- Original Message -----
From: "mata iaia" <[email protected]>
To: <[email protected]>
Sent: February 06, 2002 3:39 PM
Subject: [TheForge] Help! finish problem
>
>
> Hi all,
>
> I made a finish from a recipe of 2 parts linseed, 1 part turpintine, 3
> tablespoons japan drier, and about 4 tablespoons of beeswax.
>
> My problem is that my piece is still really tacky in some places and oily
in
> others. It has been approximately 24 hours. Did I get the recipe wrong
or
> will it just take much longer to dry? What can do if it stays sticky to
> make it dry out or thin out??
>
> Thanks,
>
> Mata
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge