> Hi all,
>
> I made a finish from a recipe of 2 parts linseed, 1 part turpintine, 3
> tablespoons japan drier, and about 4 tablespoons of beeswax.
>
> My problem is that my piece is still really tacky in some places and oily
in
> others.  It has been approximately 24 hours.  Did I get the recipe wrong
or
> will it just take much longer to dry?  What can do if it stays sticky to
> make it dry out or thin out??
>
> Thanks,
>
> Mata
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>