At 04:50 12/06/02 -0700, you wrote:
>I saw the advertisement in the recent issue of the AR for the anvils made
>by Rat Hole Forge. Can anyone comment on the quality of these
>anvils? How much do they cost?
>
>Thanks,
>
>Phil Rosche
>Summerville, SC
Phil,
I checked with the Guild of Metalsmiths and here's a reply I jut got back
tonight:
>I work at Olin Wrought Iron. Dave Olin purchased a large one at the
>conference and itworks very well. It has some good features and stands up
>well to almost
>daily use so far. And it even looks good.
>D.Feterl
Hope this helps.
Dave Brown
Heritage Smithing
Green Bay, WI