I saw them at the LaCrosse conference. Very high dollar, the big one was
over 2 grand.
I was hanging around, helping here and there during the tear down. I looked
over the Rat Hole anvil
that had been used by one of the Japanese smiths. It had some noticeable
hammer dings in the face.
At least that particular anvil was a little too soft in my opinion. It was
definitely a softer face as compared to the large Czech anvils.
This is my anecdotal observation.
Rob
----- Original Message -----
From: "Phil" <[email protected]>
To: "Forge, The" <[email protected]>
Sent: Friday, December 06, 2002 5:50 AM
Subject: [TheForge] Rat Hole Forge Anvils


> I saw the advertisement in the recent issue of the AR for the anvils made
by Rat Hole Forge.  Can anyone comment on the quality of these anvils?  How
much do they cost?
>
> Thanks,
>
> Phil Rosche
> Summerville, SC
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>