Thanks for the tip,
	I asked around a bit and there is a local swaba member, a =
retired=20
machinist, who has done die sets for other hammers for about $150 per =
set.

I uploaded a photo of the timing belt drive on my little giant to the=20
photo access site, under the tools & tooling category.



On Friday, August 9, 2002, at 12:50 PM, Gladish Family wrote:
> I took a block of tool steel (4340, HTSR, scrap from a factory) to my
> neighborhood machine shop and he made me a lower die for $60, with the =
old
> die to copy.