My ram was 6" square with 5 1/2" round welded inside, I welded some strips
down the sides of the round to pack it out a little and then just welded it
top and bottom inside the tubing, its worked fine.
 Ralph isnt it easier to put something inside the tubing instead of
attaching to the end?
----- Original Message -----
From: "John Newman" <[email protected]>
To: <[email protected]>
Sent: Monday, April 29, 2002 8:19 AM
Subject: Re: [TheForge] Air Hammer Guides


> >
>
> Thanks for all the input on the hammer guides  Today I got the support for
the
> guide tube and the guide tube welded on to the upright. Tonight I will
weld on
> the tube for the press and a cap for the top.  What I had planned to do to
hold
> the steel in the ram tube, was to V the face of the filler pc.  then weld
into
> the gap.  I will grind the face flat on a disc sander.  I may put some
dowels in
> from the sides I am using two strips of UHMW on each side so I will put
the
> dowels in between them. I don't know if this helps you or if you see
anything
> wrong with this.
>
> John Newman
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>