[TheForge] Air Hammer Guides
Ralph Sproul
[email protected]
Sun Apr 28 20:29:00 2002
Good question. I haven't done it yet as I wanted to mill the block
to fit halfway inside the tube, so maybe I should just look for another
block of steel to slide up in and weld around the edges.
I'll see what I can find in a 5 3/8 demension(or close) next time
I'm up to the fellow that carries all the cut offs from machine shops.
Ralph
----- Original Message -----
From: "Shannell Sugrue" <[email protected]>
To: <[email protected]>
Sent: Sunday, April 28, 2002 8:15 PM
Subject: Re: [TheForge] Air Hammer Guides
> My ram was 6" square with 5 1/2" round welded inside, I welded some strips
> down the sides of the round to pack it out a little and then just welded
it
> top and bottom inside the tubing, its worked fine.
> Ralph isnt it easier to put something inside the tubing instead of
> attaching to the end?
> ----- Original Message -----
> From: "John Newman" <[email protected]>
> To: <[email protected]>
> Sent: Monday, April 29, 2002 8:19 AM
> Subject: Re: [TheForge] Air Hammer Guides
>
>
> > >
> >
> > Thanks for all the input on the hammer guides Today I got the support
for
> the
> > guide tube and the guide tube welded on to the upright. Tonight I will
> weld on
> > the tube for the press and a cap for the top. What I had planned to do
to
> hold
> > the steel in the ram tube, was to V the face of the filler pc. then
weld
> into
> > the gap. I will grind the face flat on a disc sander. I may put some
> dowels in
> > from the sides I am using two strips of UHMW on each side so I will put
> the
> > dowels in between them. I don't know if this helps you or if you see
> anything
> > wrong with this.
> >
> > John Newman
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>