[TheForge] RE: burner flares

Jerry Frost [email protected]
Thu Apr 25 22:06:01 2002


The taper ratio of 1:12 is for the diameter. For example a tube starting at
1" dia would taper to a 2" dia. in 12 inches.

Ideally, yes you'd taper the entire tube for a distance of 9x the throat
diameter. The throat being the narrowest diameter of the tube (truncated
cone?)

I'm in the process of building a new forge and am experimenting with a few
burner configurations. The actual burner nozzles will be built into the
forge liner from 4,000f rammable refractory. I don't anticipate a burnout in
the foreseeable future. <grin>

Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks


----- Original Message -----
From: "Shannell" <[email protected]>
To: <[email protected]>
Sent: Thursday, April 25, 2002 5:02 PM
Subject: Re: [TheForge] RE: burner flares


> They dont taper yhe whole length though do they, I have those same flares
> but they are too melted, coroded now to measure
>