4000f rammable? Now that sounds like the stuff I've been looking for. Let us
know how it turns out. I have some old burners from a water heater from
sometime way past that I am working on using for a forge and a bronze foundry.
Could use some of that high temp refractory for it. I was hoping on doing a
similar trick for these burners as they are short but have a great built in
venturi and removable jet. As I have about a dozen, I figure I have a couple to
play with to get it right.
Larry
Jerry Frost wrote:
> The taper ratio of 1:12 is for the diameter. For example a tube starting at
> 1" dia would taper to a 2" dia. in 12 inches.
>
> Ideally, yes you'd taper the entire tube for a distance of 9x the throat
> diameter. The throat being the narrowest diameter of the tube (truncated
> cone?)
>
> I'm in the process of building a new forge and am experimenting with a few
> burner configurations. The actual burner nozzles will be built into the
> forge liner from 4,000f rammable refractory. I don't anticipate a burnout in
> the foreseeable future. <grin>
>
> Frosty