They dont taper yhe whole length though do they, I have those same flares
but they are too melted, coroded now to measure
----- Original Message -----
From: "Rick & Kims Email" <[email protected]>
To: <[email protected]>
Sent: Friday, April 26, 2002 12:50 AM
Subject: Re: [TheForge] RE: burner flares
> I had some stainless steel flares made by the guy listed at Ron Reil's
> site (can't think of his name right now). I'll see if I can get a
> measure on the angle, or the dia of the throat, mouth and the length
> in between. Then you can use your algebra skills and do some
> cypherin' (as Jethro of the Clampets used to say).
>
> Here is the info:
> Starting diameter: 1-1/16"
> Ending diameter: 1-1/8"
> Length: 3"
>
> Rick Korinek
> Emerald City Forge
> Framingham, MA
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>