bubba, line the thing with koawool first then add the castable.
then add a layer of satinite or other refractory wash to the koawool.
check out my page on gas forges
http://magichammer.freeservers.com/page9.html
and follow the links to see how
other people do it. there are a bunch of sites that have already worked out
all the problems and tell you the most efficient way to proceed.
dave m.

----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Tuesday, April 09, 2002 6:11 PM
Subject: Re: [TheForge] propane forges


> i am looking at building a propane forge using an old water heater tank (
> innards )...
> what i'm thinking about doing is pouring the bottom of the forge with a
> castable refractory and than using koawool around the rest... my idea is
this
> will keep the bottom of the forge more rigid and less likely to suffer
from
> flux break down ... hummm ... what do ya think...???
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>