its a cylinder within a cylinder. The air comes in under the floor and goes
around the out side of the inter cylinder then is pulled in though the
burners. It was a venture but only got up to 2200. so I added air now burns
at 2400+ (the pyro only goes to 2400) The preheat is about 500. next one is
going to be a bit different.  but welding at 8 PSI is not too bad
Dan Scheid
Flying horse forge
http://home.earthlink.net/~chevalvolant/flyinghorseforge.html
> Where is the exhaust to the recuperative manifold?
>
> Got a better picture or a drawing?
>
> Dave
>
> At 19:00 04/09/02 -0700, you wrote:
> >bottom one is and a recoup too,the other is not
> >Dan Scheid
> >Flying horse forge
> >http://home.earthlink.net/~chevalvolant/flyinghorseforge.html
> >
> > > Dan,
> > >
> > > Are those forced air burners?
> > >
> > > Dave
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>