I’m trying to setting up a gas-saver valve so that I can use my rosebud intermittently without having to readjust gases and relight with a spark lighter. However, the valve seems to be shutting off the acetylene first instead of the oxygen causing the torch to “pop”.. Any ideas? Is the gas saver setup backwards? Jim Smith Sent from my iPad