[TheForge] TheForge Digest, Vol 211, Issue 3

Andrew Vida impublius at gmail.com
Wed Feb 28 17:43:43 EST 2024


I second the take it apart and clean it out option for the blower.

Gouge-out/drain the bulk, then into solvent, whether Stoddard solution
(Varsol), MEK, diesel, kero, etc.  Scrup the crap out of it, get it squeaky
clean, reassemble and refill with a lighter oil whose gelling point is
low.  Actually, I'm thinking #2 Vactra way oil would be perfect for this
task, or even ATF.

On Wed, Feb 28, 2024 at 2:07 PM <theforge-request at mailman.qth.net> wrote:

> Send TheForge mailing list submissions to
>         theforge at mailman.qth.net
>
> To subscribe or unsubscribe via the World Wide Web, visit
>         http://mailman.qth.net/mailman/listinfo/theforge
> or, via email, send a message with subject or body 'help' to
>         theforge-request at mailman.qth.net
>
> You can reach the person managing the list at
>         theforge-owner at mailman.qth.net
>
> When replying, please edit your Subject line so it is more specific
> than "Re: Contents of TheForge digest..."
>
>
> Today's Topics:
>
>    1. Re: Sci-FI (Vincent Nakovics)
>    2. Re: Sci-FI (JERRY FROST)
>    3. Forge hand blower (blcksmth)
>    4. Re: Forge hand blower (J. Petrila)
>
>
> ----------------------------------------------------------------------
>
> Message: 1
> Date: Tue, 27 Feb 2024 13:32:53 +0000
> From: Vincent Nakovics <restoreman123 at msn.com>
> To: "theforge at mailman.qth.net" <theforge at mailman.qth.net>
> Subject: Re: [TheForge] Sci-FI
> Message-ID:
>         <
> IA1PR10MB68067E4B587E86E19AB616C9FF592 at IA1PR10MB6806.namprd10.prod.outlook.com
> >
>
> Content-Type: text/plain; charset="Windows-1252"
>
> No worries ? Maybe I will have to come up there and research a location
> for a murder or two. Maybe I can get my spaceship working and drop in
> quietly. hahaha
>
> Vince Nakovics
>   Author, Blacksmith, Sailor
>
> Website<https://vincenakovics.com/>
>
>
>
>
> Sent from Mail<https://go.microsoft.com/fwlink/?LinkId=550986> for Windows
>
> ________________________________
> From: theforge-bounces at mailman.qth.net <theforge-bounces at mailman.qth.net>
> on behalf of theforge-request at mailman.qth.net <
> theforge-request at mailman.qth.net>
> Sent: Monday, February 26, 2024 9:18:38 PM
> To: theforge at mailman.qth.net <theforge at mailman.qth.net>
> Subject: TheForge Digest, Vol 211, Issue 2
>
> Send TheForge mailing list submissions to
>         theforge at mailman.qth.net
>
> To subscribe or unsubscribe via the World Wide Web, visit
>         http://mailman.qth.net/mailman/listinfo/theforge
> or, via email, send a message with subject or body 'help' to
>         theforge-request at mailman.qth.net
>
> You can reach the person managing the list at
>         theforge-owner at mailman.qth.net
>
> When replying, please edit your Subject line so it is more specific
> than "Re: Contents of TheForge digest..."
>
>
> ------------------------------
>
> Message: 2
> Date: Wed, 28 Feb 2024 13:39:47 -0500 (EST)
> From: JERRY FROST <akfrosty at mtaonline.net>
> To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
> Subject: Re: [TheForge] Sci-FI
> Message-ID:
>         <117177236.22118922.1709145587198.JavaMail.zimbra at mtaonline.net>
> Content-Type: text/plain; charset=utf-8
>
> Sounds good, do I get a ride? I hope your stealth works, we have a lot of
> neighbors and we're in the landing pattern for Wasilla muni airport. If a
> person isn't an idiot disposing of bodies is pretty straight forward. Being
> a not idiot bodies don't need transporting from a city or large town of
> course. Then a can of sardines or tuna in oil will bring the bears. Body is
> now distributed in piles of bear shit. There are others though.
>
> Check out Dana Stabenow, she's a mystery author and being an Alaskan
> resident most take place here quite realistically.
>
> Jer
>
> ----- Original Message -----
> From: "Vincent Nakovics" <restoreman123 at msn.com>
> To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Tuesday, February 27, 2024 4:32:53 AM
> Subject: Re: [TheForge] Sci-FI
>
> No worries ? Maybe I will have to come up there and research a location
> for a murder or two. Maybe I can get my spaceship working and drop in
> quietly. hahaha
>
> Vince Nakovics
>   Author, Blacksmith, Sailor
>
> Website<https://vincenakovics.com/>
>
>
>
>
> Sent from Mail<https://go.microsoft.com/fwlink/?LinkId=550986> for Windows
>
>
>
> ------------------------------
>
> Message: 3
> Date: Wed, 28 Feb 2024 13:58:13 -0500
> From: blcksmth <blcksmth at reagan.com>
> To: theforge <theforge at mailman.qth.net>
> Subject: [TheForge] Forge hand blower
> Message-ID: <c3df1ee4-d63b-467b-8052-45d059938149 at reagan.com>
> Content-Type: text/plain; charset=UTF-8; format=flowed
>
>
> I have a typical forge blower that is working fine except that it is
> harder to crank than I think it should be.
> The crank is on one side of the gearbox and the fan on the other side. I
> suspect the oil has partially solidified.
> The fan is free and it does coast for a bit when you stop cranking.
> Adding oil to the gearbox has no effect.
> What would be a recommended liquid that I could pour into the gearbox to
> allow the gunk to be drained out
> and then add new oil? Gasoline comes to mind, with the usual precautions
> including a cold forge.
>
> --
>
>
> Bob Willman
> The Eagle's Anvil
> Bowling Green, Ohio
> WB8NQW
>
>
> A primary object should be the education of our youth in the science of
> government. In a republic, what species of knowledge can be equally
> important? And what duty more pressing than communicating it to those
> who are to be the future guardians of the liberties of the country?
>
>
> George Washington
>
>
>
> ------------------------------
>
> Message: 4
> Date: Wed, 28 Feb 2024 14:05:14 -0500
> From: "J. Petrila" <jlpservicesinc at gmail.com>
> To: blcksmth <blcksmth at reagan.com>,     Blacksmithing List Sponsored by
>         ABANA <theforge at mailman.qth.net>
> Subject: Re: [TheForge] Forge hand blower
> Message-ID:
>         <
> CALar+xmMN0soQJav37+4wpdshQyvwBXATG1TGASoEe23JBYgGw at mail.gmail.com>
> Content-Type: text/plain; charset="UTF-8"
>
> Kerosene or diesel..
>
> The best thing is to remove the cover and clean out the old oil..
> Sometimes there is more solid metals than expected and can damage some of
> the gears.
>
>
> JLP Services Inc
> 6 Kenwood Dr
> Rutland, MA 01543-1215
>
> 1 (508) 667-5498
>
>
> On Wed, Feb 28, 2024 at 1:58?PM blcksmth via TheForge <
> theforge at mailman.qth.net> wrote:
>
> >
> > I have a typical forge blower that is working fine except that it is
> > harder to crank than I think it should be.
> > The crank is on one side of the gearbox and the fan on the other side. I
> > suspect the oil has partially solidified.
> > The fan is free and it does coast for a bit when you stop cranking.
> > Adding oil to the gearbox has no effect.
> > What would be a recommended liquid that I could pour into the gearbox to
> > allow the gunk to be drained out
> > and then add new oil? Gasoline comes to mind, with the usual precautions
> > including a cold forge.
> >
> > --
> >
> >
> > Bob Willman
> > The Eagle's Anvil
> > Bowling Green, Ohio
> > WB8NQW
> >
> >
> > A primary object should be the education of our youth in the science of
> > government. In a republic, what species of knowledge can be equally
> > important? And what duty more pressing than communicating it to those
> > who are to be the future guardians of the liberties of the country?
> >
> >
> > George Washington
> >
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.shutterfly.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> > Message delivered to jlpservicesinc at gmail.com
> >
>
>
> ------------------------------
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
>
>
>
>
> End of TheForge Digest, Vol 211, Issue 3
> ****************************************
>


More information about the TheForge mailing list