[TheForge] Glass [TheForge Digest, Vol 213, Issue 6]

JERRY FROST akfrosty at mtaonline.net
Wed Apr 24 12:09:02 EDT 2024


I've done some slumped torch work noodle glass in forged pieces. Noodles are flat ribbon of torchwork glass rather than rods which are tiny rounds. Vermillion red in the center of spread crosses being my most successful. I've messed with some different things as well so I CAN imagine what working with molten glass in zero G would be like. A nightmare! Maybe not so much if you have the right tools but soft let alone molten glass is really sticky and draws little strings every time you do anything. Take it out of the fire, touch it to/with ANYTHING, remove the noodle, etc. and it draws strings that stick to anything break and float around the shop. The inside of my forge has a puddle that is sinking into the floor and the porch is a mess.

It's fun though.

Frosty. 

----- Original Message -----
From: "Bruce" <freemab222 at gmail.com>
To: mspencer at tallships.ca, "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, April 24, 2024 2:12:55 AM
Subject: Re: [TheForge] Glass [TheForge Digest, Vol 213, Issue 6]

We have Wheaton Arts, which celebrates the glass industry in NJ.  One
friend, a former blacksmith, has switched to flameworking and turns out
lovely marbles.  It's tempting.

Imagine what it would be like to blow glass in zero G!

Bruce
NJ


On Wed, Apr 24, 2024 at 2:17 AM Mike Spencer <mspencer at tallships.ca> wrote:

>
> Mark> Always wanted to work with glass.
>
> Dick> I added glass blowing about 13 years ago on top of the 38 years
> Dick> of blacksmithing. I play with glass more often than iron these
> Dick> days.
>
> I hitched a ride home from the 1976 ABANA con with a couple who were
> keen to see the Blenko glass works in W. Virginia.  It was worth
> the extra day on the roak to visit the works.
>
> About that same time, I did a 3-day public demo adjunct to a craft
> market.  They set me up in a fire-safe, wind-protected patio and put
> the glass blower there too.  During the weekend, I forged a little
> basket affair and he blew a bottle into it.  Regrettably, we stood
> around admiring or work for too long, failed to get it into the
> annealing oven soon enough so it went PING and fell apart.
>
> He gave me some basic instruction, let me mess about a bit.
> Observation:  A blacksmith doggedly pushes the iron, inch by inch,
> millimeter by millimeter, where (s)he wants it to go.  With hot glass,
> you're constantly chasing after the gather/workpiece as it tries, in
> conspiracy with gravity, to run away from you.
>
> --
> Michael Spencer                  Nova Scotia, Canada       .~.
>                                                            /V\
> mspencer at tallships.ca                                     /( )\
> http://home.tallships.ca/mspencer/                        ^^-^^
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to freemab222 at gmail.com
>
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
Message delivered to akfrosty at mtaonline.net


More information about the TheForge mailing list