[TheForge] ITC-100HTi from their web site

terry l. ridder terrylr at blauedonau.com
Mon Mar 29 20:24:21 EDT 2021


Hello

I purchased a gallon of itc100. I paid $190.00 USD for the gallon.
I have never had any issues with itc100ht.

Currently a pint cost $49.99 USD

Here from the ITC web site is what I go by.

About ITC Coatings
OUR MISSION:

To be the leading provider of technical ceramic coatings to help producers
and manufacturers protect their equipment from heat, wear and corrosion,
while significantly reducing energy costs, emissions and maintenance.
Our aim is to always deliver the highest quality products and service to our
customers.

ITC Coatings are high-temperature ceramic coatings for kilns, forges,
furnaces, ovens and metal equipment. Our high-reflectivity coatings
increase the efficiency of firing equipment and protect refractory and
metal surfaces from heat, wear and corrosion.

The ITC line of coatings were developed in 1980 in Alliance, Ohio by
Feriz Delkic, a ceramic engineer who was running his own pottery business
at the time. He created the coatings as a solution to the crippling costs
of operating and maintain his kilns. After applying the first original
formula - now known as ITC 100HT -  to the interior lining of his kilns,
he saw his energy bills decrease by more than 60%.

Upon seeing a consistent sizeable reduction of their utility bills,
Feriz’s wife Alice suggested their efforts would be better spent
helping other businesses facing similar issues, and International
Technical Ceramics, Inc. was formed. Since then, ITC Coatings have
been providing solutions to problems faced by major companies in
industries such as Steel, Power Generation, Petrochemical, Cement,
Brick and Tile Manufacturing, as well as ceramic artists and home
hobbyists all over the world.

ITC Ceramic Coatings are a versatile line of high temperature technical
industrial coatings that protect and maintain all types of refractory
and metal equipment in some of the harshest industrial environments,
while also increasing production efficiencies and product quality.
ITC Coatings contain no volatile organic compounds, are not harmful
to the environment and even help reduce toxic emissions in many
instances.

Contact us to learn how ITC Coatings can help you protect your equipment,
improve your process, decrease maintenance and provide considerable savings
to your business
                                                                                                                    1,1
<begin quote>
https://www.itccoatings.com/knifemaking

ITC Coatings have proven to be an absolute necessity for knifemakers,
metalworkers and other hobbyists and craftsmen looking to get the most
out of their forging operation. With high temperature capacity and
durability, ITC Ceramic Coatings are able to withstand the harsh
environments that forge owners and operators face on a daily basis.

Because ITC Ceramic Coatings reflect almost all heat (90-98%) on the
radiation spectrum, your forge heats will heat up more rapidly. In
addition, the heat from the burner is retained in the forge for a
longer period of time. Not only does this allow for greatly reduced
consumption of fuel by the forge, but it also reduces the amount of
heat being soaked into the lining. This both protects and extends the
life of the refractory lining, as well as provides a more even heat
throughout the forge. When it's time to shut down the forge, the heat
can dissipate more quickly, since the forge lining is not soaking up
all the heat.

ITC Ceramic Coatings protect forge refractory and knife making equipment
from the harsh environments to which they are exposed. ITC Ceramic Coatings
can come into contact with molten metal without being destroyed, providing
longer life for tools used in the knifemaking and metalworking processes.
ITC Ceramic Coatings can also withstand damaging flux and corrosive agents
that attack and destroy forge linings and metalworking equipment.

ITC 100HT Ceramic Coating

The absolute workhorse in forge lining protection and efficiency. 100 HT
can handle the highest temperatures and help reduce fuel consumption by
up to 50%. Achieve reduced firing times and more even heats for a better
quality product.

iTC 100HT Ceramic Coating

The absolute workhorse in forge lining protection and efficiency. 100 HT
can handle the highest temperatures and help reduce fuel consumption by
up to 50%. Achieve reduced firing times and more even heats for a better
quality product.


ITC 296A Ceramic Top Coat

With a very high temperature rating and a low porosity, 296A is very
effective as an added layer of protection to protect brick and fiber
refractory from build-up and corrosive agents, further improving forge
efficiency.
Learn More https://www.itccoatings.com/ceramic-coating

ITC 148 Heavy Duty Ceramic Repair

A putty-like abrasion-resistant compound for repairing areas exposed to
harsh environments and mechanical abuse. Great for tools, walls and
floors
in contact with molten metal.

For Technical support and questions about materials,
applications and quantities:
Greg Odenthal
412.498.7270
greg at itccoatings.com


For ordering info and General inquiries:
817.337.9889
office at itccoatings.com

-- 

terry l. ridder ><>


More information about the TheForge mailing list