[TheForge] Price
Dave Mudge
davemudge1 at gmail.com
Sat Feb 20 15:33:36 EST 2021
The 1035 is 5-1/4" square...
On Sat, Feb 20, 2021, 1:43 PM Dave Mudge <davemudge1 at gmail.com> wrote:
> Seeking advice of our well informed members.
> I have a piece of 4340,, 4"sq. 44" long. And a piece of 1035 double melt
> crucible steel 36" long all good for power hammer dies. A friend wants to
> buy one or both. What are each one worth?
> dave m