Think denatured ETOH for hand cleaning - a gallon from the box store {paint aisle} goes a long way - diluted 3:7. Incidentally, the small insect repellent spray bottles make decent delivery devices. Better than 'think good thoughts' <grin>
Steve
________________________________
From: theforge-bounces at mailman.qth.net <theforge-bounces at mailman.qth.net> on behalf of Bruce . <freemab222 at gmail.com>
Sent: Saturday, March 28, 2020 8:56 PM
To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Subject: Re: [TheForge] Copper vs. coronavirus
Changing the subject a bit: I went shopping today (garbed in a light
raincoat, homemade mask, plastic visor and broad-brimmed hat!). One stop
was the liquor store. I'm not a big drinker but like to have a choice:
wine, beer, or high-test, namely Everclear (which is the cheapest alcohol
around, 190 proof). Normally I buy the Everclear in the 1.75 liter bottle,
as it's significantly cheaper than smaller sizes (and it keeps forever).
Today, that size was sold out -- the first time EVER I've seen it sold
out. I guess either folks are getting plastered while staying home, or
else it's being used for hand sanitizer. (I'd rather use soap!)
Bruce
NJ
On Sat, Mar 28, 2020 at 8:29 PM jerry Frost <akfrosty at mtaonline.net> wrote:
> Hmmmm, maybe, maybe not. Here's an article from a site I often read
> regarding antiseptic copper with cites and links to original research
> papers and material.
>
> Frosty
>
> https://www.sciencedaily.com/releases/2015/11/151110102147.htm
>
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net [mailto:
> theforge-bounces at mailman.qth.net] On Behalf Of Walter
> Sent: Friday, March 27, 2020 8:44 AM
> To: theforge
> Subject: [TheForge] Copper vs. coronavirus
>
> This is an interesting thread.
>
> Regarding face masks. The hand sewn face masks that volunteers are making
> are worthless in protecting the user from the virus because a virus is so
> small that it goes through the openings. The N95 mask works because the
> mesh in it is super fine. It also has to seal against the face so beards
> should be shaved to use them. (Not too good for many of we smiths.)
>
> Therefore, copper ions in the fabric is probably not a solution.
>
> Stay safe so stay at home.
>
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to freemab222 at gmail.com
>
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
Message delivered to sabloom at ironflower.com
More information about the TheForge
mailing list