[TheForge] Band Saw Blade
LAWRENCE BROWN
lp.brown at verizon.net
Sun Dec 20 19:04:26 EST 2020
Best way is to find someone with the welder attachment on their saw, after that I have mig welded then ground and lightly annealed, tig welded but the set up couldn’t be turned down enough, brazed and silver soldered. The mig yielded the longest lasting results of what I tried. I had a friend with the blade welder at work make me a few and they lasted well, but that shop closed. You can buy the blades from vendors cut and welded to size which is what I did the last few blades I needed
Larry Brown
> On Dec 18, 2020, at 7:41 AM, J. Petrila <jlpservicesinc at gmail.com> wrote:
>
> there are several ways.. the easiest but most expensive is to by a bandsaw
> blade welder.. they can be priced from about 500.00-10k
>
> You can tig weld them if you are really good and then anneal them in free
> air.
>
> You can also silver solder them and they sell units to hold the blades so
> this can be done.
>
> I own 2 bandsaw blade welders and is a great investment if using them
> enough or if you want to do internal cutting.
> JLP Services Inc
> 6 Kenwood Dr
> Rutland, MA 01543-1215
>
> 1 (508) 667-5498
>
>
> On Fri, Dec 18, 2020 at 1:00 AM Dave Mudge <davemudge1 at gmail.com <mailto:davemudge1 at gmail.com>> wrote:
>
>> Good evening group, Merry Christmas and Happy New Year.
>> I was given a coil of band saw blade material.
>> Metal cutting, 1/2" wide. When I cut pieces to
>> the length I need, How do I weld the joint?
>>
>> dave m
>> your Listmom
>>
>> --
>>
>> ...sometimes you're the windshield,
>>
>> ...sometimes you're the bug
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.shutterfly.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>> Message delivered to jlpservicesinc at gmail.com <mailto:jlpservicesinc at gmail.com>
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge <http://mailman.qth.net/mailman/listinfo/theforge>
> Help: http://mailman.qth.net/mmfaq.htm <http://mailman.qth.net/mmfaq.htm>
> Post: mailto:TheForge at mailman.qth.net <mailto:TheForge at mailman.qth.net>
>
> TheForge mail list group photo site is
> http://www.shutterfly.com <http://www.shutterfly.com/>
> Login: blacksmithblacksmith at hotmail.com <mailto:blacksmithblacksmith at hotmail.com>
> Password: anvil
>
> This list hosted by: http://www.qsl.net <http://www.qsl.net/>
> Please help support this email list: http://www.qsl.net/donate.html <http://www.qsl.net/donate.html>
> Message delivered to lp.brown at verizon.net <mailto:lp.brown at verizon.net>
More information about the TheForge
mailing list