[TheForge] 50 Pound Little giant
Steve Bloom
sabloom at ironflower.com
Tue Oct 22 12:28:08 EDT 2019
On 10/22/2019 9:48 AM, Daniel Kretchmar wrote:
> Will a 5 hp compressor motor work?
way overkill but if you have it.....<grin>
Specs on my 50 lb Little Giant - in service since 1991. Motor is a
Marathon cat.No-Z118. 1.5 HP 1725 rpm 220V Farm Duty TEFC. The pulley
is 3.25" diameter and runs two V-belts.
In that time, I have had the motor overheat twice - when ambient temp
was 100F and while running Damascus forge full bore. The forge is maybe
18" lower and 12" to the left of the motor and is a dual burner, rear
vent system.
Of course, one of the first rules about mechanic hammers is that there
is never anything like too much oil. Good luck with your beast - I
can't imagine not having one when I need it!
steve
More information about the TheForge
mailing list