You beat me to it. I have used naval jelly, electrolysis, sandblasting, acid, wire brush over the years, but tried evaporust recently and am sold. I will say that I have evolved to using wire brush or sandblast first and then dunking it in the evaporust because there is a finite amount of rust that the evaporust will absorb. As you stated it uses chelation, which means the evaporust binds tightly to oxidized iron and pulls it into solution. Eventually the solution will become saturated and it no longer works. You will see it slow down over time. The benefit for me of evaporust is that it gets into all of the small spaces that a sandblaster or wire brush can't. It even excels over electrolysis in this aspect since electrolysis depends on line of sight between the cathode and anode to an extent. I will also add that a bucket of marbles is useful in that they can be used to raise or lower the level of evaporust solution to cover the item at hand without buying more. It is not cheap.
Charles On Wednesday, March 6, 2019, 10:59:46 AM CST, Chuck Robinson <robi5515 at bellsouth.net> wrote:
Hey Dave,
The best cleaner I have used is Evaporust, available at Harbor Freight.
Item # 96431
It uses a chelation process to remove only the rust. It is nontoxic,
easy to use, and is a neutral liquid.
After a lot of use, let the rust settle in the bottom of the container
and then decant the clear liquid and it is ready for more use.
Chuck
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list