[TheForge] fixed broken link was Re: fish plates? just how big are they?

J. Petrila jlpservicesinc at gmail.com
Fri Jun 23 18:36:30 EDT 2017


That there is a mighty easy fix.. I was actually able to view it this
time... Thanks..  I would clean the heck out of it. Lay a fillet weld in
there and if the need strikes me I would add a small gusset to each side..
  That's a really easy fix.. Clean, Clean, Clean is the key..

JLP Services Inc
6 Kenwood Dr
Rutland, MA 01543-1215

1 (508) 667-5498

On Fri, Jun 23, 2017 at 1:16 PM, terry l. ridder <terrylr at blauedonau.com>
wrote:

> hello
>
> i have moved the photographs of the broken weld
> to neubach.blauedonau.com/~terrylr/weld/
>
> i have checked the link from several different networks and the link
> does work.
>
> On Fri, 23 Jun 2017, terry l. ridder wrote:
>
> hello
>>
>> I did post photographs of the broken weld in my first post on the
>> subject.
>> the photographs were uploaded to my web server on my linux laptop.
>> birnbaum.blauedonau.com/terrylr/ or
>> 204.238.34.132/terrylr/
>>
>> there appears to be an issue with 'birnbaum.blauedonau.com' dns
>>
>> there are three photographs listed.
>> the photographs are self-explanatory.
>>
>>
> --
> terry l. ridder ><>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to jlpservicesinc at gmail.com
>


More information about the TheForge mailing list