[TheForge] broken weld on mower deck
J. Petrila
jlpservicesinc at gmail.com
Tue Jun 6 14:01:42 EDT 2017
do it cold.. If it bent cold, bend it back cold.. If the parts are worn
from surface abrasion then add a new patch in..
Mig welding, A/O is perfect or tig welded depending on what kind of fix..
MIg or Tig will give you the least clean up before repainting..
I've fixed maybe 20 mower decks with wheels and supports knocked off or
bent.. Not one of them was a simple straight forwards fix..
Each one needed to be slit here or there and then massaged back into
position before final welding..
I couldn't bring the pictures up but overall it's a pretty straight
forwards job unless it's been ran over by a Mack truck..
JLP Services Inc
6 Kenwood Dr
Rutland, MA 01543-1215
1 (508) 667-5498
On Tue, Jun 6, 2017 at 1:38 PM, terry l. ridder <terrylr at blauedonau.com>
wrote:
> hgello
>
> the left front scalp wheel on a kubota mower deck has broken the welds.
> i have upload two photographs of the broken welds at:
> birnbaum.blauedonau.com/terrylr
>
> birnbaum, my new linux laptop.
>
> my concern is that when i bring the parts back together the remaining
> weld is going to break. Should I heat the parts to make them a little
> more amenable to moving back into place?
> I do not have a stick welder so I need to use either the mig welder or
> the oxy-act torch. I would rather use the mig welder.
>
> any suggestions, hints, welcomed.
>
>
> --
> terry l. ridder ><>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to jlpservicesinc at gmail.com
>
More information about the TheForge
mailing list