[TheForge] Foil/sheet/plate

J. Petrila jlpservicesinc at gmail.com
Tue Jul 4 07:25:08 EDT 2017


They make foil in many different types..  Stainless steel foil is used for
hardening different steels and alloys.. It is made into an air tight
package or envelope sometimes with different materials to change the
environment inside the package..

This will keep the tool scale free..

JLP Services Inc
6 Kenwood Dr
Rutland, MA 01543-1215

1 (508) 667-5498

On Tue, Jul 4, 2017 at 1:44 AM, Mike Spencer <mspencer at tallships.ca> wrote:

>
> Dave Smucker <davesmucker at hotmail.com> wrote:
>
> > In ferrous metal there is very little foil produced since it becomes
> > so hard to roll at very light gauges.  There are some special
> > products for which it is produced in foil gauges but very expensive.
>
> Somewhere I have a piece of stainless thin enough that I'd call it
> foil.  Don't have a number but easily flexible with the fingers, about
> the same thickness as an Al 11x14 photo offset plate or maybe a tad
> less.
>
> No idea what it may have cost.  Someone gave it to me, maybe at an
> ABANA conference or NEB meet years ago.
>
> What can you tell us about making that?  Seems like a hard go, given
> what you've said:
>
> > The technical reason for this is that as the metal gets very thin the
> > rolls flatten rather that the metal being rolled.
>
>
> - Mike
>
> --
> Michael Spencer                  Nova Scotia, Canada       .~.
>                                                            /V\
> mspencer at tallships.ca                                     /( )\
> http://home.tallships.ca/mspencer/                        ^^-^^
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to jlpservicesinc at gmail.com
>


More information about the TheForge mailing list