You can use a break drum for the fire pot. Weld the lug holes shut and
weld a steel flange over the center hole. Make the flange 2" or
larger. That way the down pipe Tee and air and dump pipe can be
removed for transport.
On 8/25/16, Ron Childers <ron at munlaw.net> wrote:
> Are you fabricating a firepot? You could weld short sections of 3/4" pipe to
> the box and use 1/2" pipe for the legs so it can be taken apart. Beware
> when welding anything galvanized; zinc fumes can make you ill ~~~~><>
>
> -----Original Message-----
> From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of
> McKenzie Miller
> Sent: Thursday, August 25, 2016 4:49 PM
> To: theforge at mailman.qth.net
> Subject: [TheForge] New to this
>
>
> I'm a PA college student welding engineering major, and I'm making a hobby
> backyard sized coal forge for my Capstone project, and I'm not sure on the
> fire box sizing and over all table size (needs to fit in the trunk of a
> compact vehicle). Any help or suggestions would be appreciated
>
>
> Sent from my Verizon Wireless 4G LTE smartphone
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html Message
> delivered to ron at munlaw.net
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to klgeorge at kent.edu
>
--
Kim George
"Why for you try to bury me in cold,cold ground?"
Taz
More information about the TheForge
mailing list