I use a 16oz ball pein on large, over 5/16" iron rivets. Does a treadle
hammer rivet set save a lot of time?
Sorry Pete I couldn't help it. <snicker>
Jer
-----Original Message-----
From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Peter
Fels & Phoebe Palmer
Sent: Sunday, March 1, 2015 8:20 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Rivet question
Thanks Jerry and Bob.
Yeah, got impatient and used the treadle hammer to rough set it in.
On Mar 1, 2015, at 8:20 PM, Bob Ehrenberger <eforge at centurytel.net> wrote:
From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Peter
Fels & Phoebe Palmer
Sent: Sunday, March 1, 2015 2:20 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Test
OK.BS question:
I was assembling one of my jointed bottle openers ( one that i had to take
back apart and forge on some more to get the parts to work right), and after
i'd set down and headed the 1/4" brass rivet, i had to spend 15 minutes
wiggling it back and forth to free it up.
Both holes were hot punched and the mating surfaces were hand forged so
nothing was accurately aligned.
What's the best, quickest way to keep the parts moving freely after the
rivet is set down?
-- Reply---
The best thing is to prevent the rivet from getting too tight in the first
place.
If you put a piece of card stock between the parts before riveting you can
remove it after riveting and there should be some clearance. Also when
setting the rivet the lighter the hammer you use the easier it is to keep
the upset at the very end.
Bob Ehrenberger
Shelbyville, MO
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list