Ya'll need to check out MG750 rods. Not as expensive, great for dissimilar
steels, NO pre/post heat. Been using them for years for mild hardy tangs to
tool steel, and anvil repair.

It's not firewood, it's a vaasse.
Dan Tull
Georgia

On Wed, Jun 3, 2015 at 8:29 PM, jerry Frost <akfrosty at mtaonline.net> wrote:

> Good deal, I think you're on the right track now.
>
> I use Kaowool, refractory ceramic blanket for annealing if I don't just
> leave it in the forge till cool. Great stuff, I keep extra around just
> because.
>
> Frosty
>
> -----Original Message-----
> From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Mike
> Spencer
> Sent: Wednesday, June 3, 2015 3:15 PM
> To: theforge at mailman.qth.net
> Subject: [TheForge] Arc welding advice sought
>
>
> Follow-up to my problem of brittleness & fracture in the HAZ when welding
> m/s to truck helper spring stock:
>
>    + Cut off a test piece of the stock.
>
>    + Pre-heated in gas forge.  Turned kinda purple-ish but not a
>      carefully controlled heat.
>
>    + Welded while hot with 7018.  Just a butt weld, no V but reversed
>      polarity.
>
>    + Post-heated in gas forge.
>
>    + Wrapped in ceramic wool batts until dead cold.
>
> Once cool, I put the test piece in a heavy vise and tried to bust it with a
> 12# sledge.  No sign of cracking.
>
> So today I repeated the process with the actual work piece.  Almost too big
> for the tube-type forge but I git it in and turned around several times.
> The m/s part was already tacked in place and it got dull red but not the
> much heavier 2x3x8 inch spring stock.
>
> It'll take all night for it to cool in the batts so we'll see tomorrow.
>
> An aside: That ceramic batt is great stuff. Set a hot workpiece on it so
> the
> welding table won't draw heat.  Lay a piece over the top and you can rest
> your gloved hand on the hot workpiece without getting burned.
>
> Thanks all for the suggestions,
> - Mike
>
> --
> Michael Spencer                  Nova Scotia, Canada       .~.
>                                                            /V\
> mspencer at tallships.ca                                     /( )\
> http://home.tallships.ca/mspencer/                        ^^-^^
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list