how bout about using casting investment?
On Apr 22, 2015, at 3:10 PM, jerry Frost <akfrosty at mtaonline.net> wrote:
I haven't tried that it's on the schedule now for sure. I'm melting frit or
noodles not cut glass. I think cutting the kiln paper as a plug has more
promise than anything I've tried seen so far.
Thank you.
Jer
-----Original Message-----
From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of
mondloch at silvercreekpottery.com
Sent: Wednesday, April 22, 2015 12:41 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Floating glass to back.
Have you tried cutting a piece kiln paper that fits tight in the bottom of
the void with another larger piece under? Cut the glass so the fit is close
so you don't have to fire quite as high.
-----Original Message-----
From: jerry Frost
Sent: Wednesday, April 22, 2015 1:30 PM
To: 'Blacksmithing List Sponsored by ABANA'
Subject: [TheForge] Floating glass to back.
Tin's SG is 7.3 and steel's SG is 7.8 so floating is no joy. Mild steel
won't float on molten tin. It's possible to come up with a stand to support
the cross's bottom surface just below the surface of the tin. The problem
then is freeing the piece from the tin once it's cooled. Tempering
(annealing) the glass takes considerable time and isn't finished till it's
cool. Also, I don't want to "tin" the cross.
Possible but maybe not practical. I'll put floating with tin in the maybe
files unless the kiln paper doesn't work or one of the art glass people
don't have a better alternative.
Thanks again guys. I LOVE brainstorming.
Jer
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list