Remember a Smooth transition fitting. This might diminish savings on pipe.
You using black pipe or something pricey to start out with?
We have convinced all those whose pipes we would replace every two years
to let us make stainless 24 ga pipe for them.
Most of them are in now better than twelve years.
Not so good for us, much better for them. It easily paid for our service
calls to replace the pipes.
Mike Graf
On 11/7/2014 8:23 PM, Andrew Vida wrote:
> I will make this quick - same friend needs to put in flue for her wood
> stove, which has a 7" flange. She is thinking of putting in a 6" flue
> because of costs. Is this rational? I've not been a big fan of choking
> down the designed flow of such devices, but the manufacturer (Hitzer)
> says while not optimal, it is OK.
>
> Opinions?
>
> Thanks.
>
> -Andy
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list