Rigidized is the main supplier of textured sheet. They usually stock stainless, but will do aluminum.
Its incredibly expensive to tool up to do this- gigantic rolling machines, with machined rolls for each texture that are 50" or so wide, and easily tens of thousands of dollars per pattern. As a result, almost every supplier you find online just buys it from Rigidized, and marks it up.
I have been buying direct from them for 25 years now.
Its great stuff, but its not cheap- especially because it needs to be palletized and shipped by truck.
http://www.rigidized.com/
ries
On Mar 27, 2014, at 6:15 AM, Dave Mudge wrote:
> Good Morning Group,
> I am looking for a source for pre-hammered sheet aluminum (or even
> stainless)
> about in the 18 gauge to 20 gauge thickness. It's for a possible project
> through
> the shop where I work. The client's budget probably wouldn't cover hand
> hammering or
> even powerhammer working the sheet.
>
> thanks,
> dave m
> --
>
>
>
>
>
>
>
>
>
>
>
> NOTICE: Due to Presidential Executive Orders, the National Security Agency
> may have read this email without warning, warrant, or notice. They may do
> this without any judicial or legislative oversight. You have no recourse
> nor protection.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
Ries Niemi
Industrial Artist
WWW.RiesNiemi.com
More information about the TheForge
mailing list