Peter,
Tempil sticks might work better for you task.
Bruce
NJ
On Sun, Dec 7, 2014 at 12:56 AM, Peter Fels & Phoebe Palmer <
artgawk at thegrid.net> wrote:
> I have been forging different bronzes that of course have differing
> forging heat ranges.
> So i got one with a wider temp range, thinking it would help with that..
> But it’s sometimes slow to read, which doesn’t work with smaller pieces
> that cool quickly.
> Also, differing levels of surface oxides seem to confuse it…
> And it keeps changing it’s digital mind.
> It did better when i was keeping track of interpass temperatures and
> carbon steel tempering.
>
> On Dec 6, 2014, at 9:33 PM, Dave Mudge <dave at magichammer.net> wrote:
>
> Bruce, our machine shop bought one of those several years ago.
> it seems to work great. Still has the same batteries...
> dave m
>
> On Fri, Dec 5, 2014 at 7:59 PM, Bruce . <freemab222 at gmail.com> wrote:
>
> > Speaking of HF tools, here's one that I've found to be reliable and
> > reasonably accurate. I've just been using mine to test pre-heat temp
> > (~400F) for welding. I may stop by the store for a second one.
> >
> > http://www.harborfreight.com/
> > item 69465
> >
> > It looks like the sale is on-line only, but sometimes the stores will
> honor
> > it if you bring the ad.
> >
> > That freebie flashlight is also a good one. I was just using one of
> mine.
> > It has a hook on the back to hang from a nail, and switches between
> > flashlight and "lantern" modes.
> >
> > Bruce
> > NJ
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.shutterfly.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> >
>
>
>
> --
>
>
>
>
>
>
>
>
>
>
>
> NOTICE: Due to Presidential Executive Orders, the National Security Agency
> may have read this email without warning, warrant, or notice. They may do
> this without any judicial or legislative oversight. You have no recourse
> nor protection.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list