Well I adapted my venture burners with a fan . upped the jet size and
lowered the PSI I was getting 2350 ish at 15#  I got 2200 at 8# no fan in 5
minute warm-up and pinged the meter at 10 minutes with fan (meter goes to
2400) put a chunk of scrap Damascus in and it was past welding heat in no
time.  S I want to thank Steve and jerr and others for their input it worked
.. now I just need to buy fuel. 
Dan Scheid