On 9/5/2013 9:47 AM, Vincent Nakovics wrote:
> Hi All,
> I find myself having to build a forge for Charcoal and with the available materials I believe the use of a side blower would be best. I will not be
> able to obtain a cast fire pot. The thickess of material reasonably
> obtained will be about 1/4" x 2" to make a pot out of. I know with a coke forge I had that material get to hot in the past. That is why I am thinking a side blower. This is a more primitive unit than I have made or used in the past so I have a couple of questions.
>
> 1. Does the insulating material in the forge have to be sand or can it be dirt?
> 2. Clinker forming at the nozzle is just raked off as all forges?
> 3. Depth of insulating layer of sand and dirt? I plan on using a metal pan, but may have to resort to a wooden box. I do not have any building enforcement codes to contend with here, but I do want a safe forge.
> 4. Any other advise please greatly appreciated.
>
> Thank you in advance!!!
>
> Vince Nakovics
>
> Blacksmithing; “Making exquisitely simple items extraordinary and tremendously complex items understatedly simple”.
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
Vince I have and other guys that I know that do 18th cen. liveing
history with have used good clay that we dug out of the ground mine was
some good blue clay that came out of a hole dug for a new house bsament
has held up for 10 years or so Jim O.