Paul,
Thanks. I'm glad it works good. Is it expensive?

Rob

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Paul Sperbeck
Sent: Saturday, February 16, 2013 3:40 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Evapo-RustR De-Rusting Solution

I use it and love it. It will not eat steel or iron, only iron oxides. 
Never tried it for stripping old bluing, but I think that would work as
well.
I have heard there are some knock offs and have heard that they do not work
as well. Stick with the Evaporust and you will not be disappointed.
It use to be available at Horror Fright as well. They do carry other than
store brand stuff... just make sure it says Evaporust

paul

No trees were killed in the generation of this message, but a tremendous
number of electrons were terribly inconvenienced

Try to notice the thing that happened just before the thing you didn't want
to have happen happened!

If you are using violence and it does not work, You are not using enough.

Life's tough, pilgrim, and it's even tougher if you're stupid. - John Wayne

Resistance Is Not Futile!  It's voltage divided by current.




On 02/16/2013 03:09 PM, Rob Fertner wrote:
> Here's another interesting product. This one I would have real use for.
> Has anyone used this or has knowledge of it? I'd like to know if this 
> stuff really works.
>
> http://www.daubertcromwell.com/evaporust.asp
> <<snip>>

______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list