I would not use concrete for the base...hot metal on concrete has been
known to make the concrete explode. I have a tendancy to set things down on
the anvil table for a moment when I need to adjust my grip.
On Mon, Aug 26, 2013 at 5:29 PM, Carrie Haag <grddog85 at gmail.com> wrote:
> Dan, my interest in smithing is along the lines of functional art (pot
> racks, utensils, etc). As much as I love renfaires reenactment isn't
> something I'm all that interested in, smithing in a corset sounds
> dangerous.
>
>
> On Mon, Aug 26, 2013 at 4:04 PM, Dan Scheid <damales at pollybutte.net>
> wrote:
>
> > As said fire tools , what are your interests reenactment , art? ,
> > functional
> > ? just like to hit steel? . make what you wish lack of horn will matter
> > little. practice welding in my book this is to skill learn early. I
> learned
> > it the second day in school. Upseting another useful skill to master.
> Play
> > hard and make shit... err stuff
> > Dan Scheid
> > -----Original Message-----
> > From: theforge-bounces at mailman.qth.net
> > [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Carrie Haag
> > Sent: Monday, August 26, 2013 10:53 AM
> > To: Blacksmithing List Sponsored by ABANA
> > Subject: [TheForge] Advice for a beginner.
> >
> > I'm planning on starting my coal forge up for the first time in about a
> > month. I think I have enough coal for a small project. I've made an "s"
> > hook and a rather ugly leaf with the over site of a much more experienced
> > smith. I have a piece of rail road track, a forge, a cross pein hammer,
> a
> > pair of vice grips, and a ton of rebar (not ideal I know but better than
> > nothing for a beginner). As the RR track doesn't have a horn I don't
> think
> > I can make an "s" hook. What projects would be a good starting point for
> > the experience and equipment I have?
> >
> > --
> > Carrie Haag
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.shutterfly.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> >
> >
> > -----
> > No virus found in this message.
> > Checked by AVG - www.avg.com
> > Version: 2013.0.3392 / Virus Database: 3211/6610 - Release Date: 08/26/13
> >
> > -----
> > No virus found in this message.
> > Checked by AVG - www.avg.com
> > Version: 2013.0.3392 / Virus Database: 3211/6607 - Release Date: 08/25/13
> >
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.shutterfly.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> >
>
>
>
> --
> Carrie Haag
>
> "If we shadows have offended, think but this, and all is mended- that you
> have but slumb'red here while these visions did appear." ---Shakespeare
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list