I have a Trenton that's well over a century old, it has an unusual base
that makes it perhaps a collector piece. First decent anvil I had.
When I got it the off side was pretty chewed up and one day I took some
stainless stick rod and just built the edge up to suit me. Have done a
world of work on it since...not the best material to use, but if the object
is to have a good, working anvil with the edges you need to get the job
done, what's to lose?
Never regretted it, though I agonized over it at the time.